Cold rolled steel rust protection oil ISO 22

(submitted by the website administration)

Cold rolled steel rust protection oil ISO 22
Mineral based oil with corrosion inhibitor
Property Value in metric unit Value in US unit
Density at 60°F (15.6°C) 0.880 *10³ kg/m³ 54.9 lb/ft³
Kinematic viscosity at 104°F (40°C) 20.5 cSt 20.5 cSt
Kinematic viscosity at 212°F (100°C) 4.0 cSt 4.0 cSt
Flash Point 190 ºC 374 ºF
Coverage 41.7 m²/l 1700 ft²/gal

Applications: colled rolled sheets and coiled strips during storage and transportation.