Semi-synthetic compressor oil ISO 100

(submitted by the website administration)

Semi-synthetic compressor oil ISO 100
Semi-synthetic oil
Property Value in metric unit Value in US unit
Density at 60°F (15.6°C) 0.870 *10³ kg/m³ 54.3 lb/ft³
Kinematic viscosity at 104°F (40°C) 96.7 cSt 96.7 cSt
Kinematic viscosity at 212°F (100°C) 11.7 cSt 11.7 cSt
Viscosity index 110 110
Flash point 248 ºC 478 ºF
Pour Point -30 ºC -22 ºF

Applications: stationary and portable screw compressors.