Stainless steel AISI 410

(submitted by the website administration)

AISI 410
Chemical composition: C=0.15%max, Mn=1%max, Cr=12.5%
Property Value in metric unit Value in US unit
Density 7.7 *10³ kg/m³ 481 lb/ft³
Modulus of elasticity 200 GPa 29000 ksi
Thermal expansion (20 ºC) 9.9*10-6 ºCˉ¹ 5.5*10-6 in/(in* ºF)
Specific heat capacity 460 J/(kg*K) 0.11 BTU/(lb*ºF)
Thermal conductivity 24.9 W/(m*K) 173 BTU*in/(hr*ft²*ºF)
Electric resistivity 5.7*10-7 Ohm*m 5.7*10-5 Ohm*cm
Tensile strength (annealed) 520 MPa 75400 psi
Yield strength (annealed) 275 MPa 40000 psi
Elongation (annealed) 30 % 30 %
Hardness (annealed) 82 RB 82 RB
Tensile strength (cold drawn) 834 MPa 121000 psi
Yield strength (cold drawn) 721 MPa 105000 psi
Elongation (cold drawn) 21 % 21 %
Hardness (cold drawn) 24 RC 24 RC