Titanium β-alloy Ti-15V-3Cr-3Sn-3Al
Chemical composition: O=0.13% max., V=15%, Cr=3%, Sn=3%, Al=3%, Ti balance
Property Value in metric unit Value in US unit
Density 4.17*10³ kg/m³ 260 lb/ft³
Modulus of elasticity 103 GPa 15000 ksi
Thermal expansion (20 ºC) 9.7*10-6 ºCˉ¹ 5.4*10-6 in/(in* ºF)
Specific heat capacity 500 J/(kg*K) 0.12 BTU/(lb*ºF)
Thermal conductivity 8.1 W/(m*K) 56 BTU*in/(hr*ft²*ºF)
Electric resistivity 147*10-8 Ohm*m 147*10-6 Ohm*cm
Tensile strength 1131 MPa 164000 psi
Yield strength 1035 MPa 150000 psi
Elongation 11 % 11 %
Solution temperature 800 ºC 1475 ºF
Aging temperature 538 ºC 1000 ºF
Aging time 8 hrs. 8 hrs.
Melting temperature 1524 ºC 2775 ºF
Beta Transus temperature 760 ºC 1400 ºF