to Ceramic Matrix Composites (introduction)
to Properties of composites

Carbon-Carbon Composite (randomly oriented fibers)

(submitted by the website administration)

Carbon-Carbon Composite (randomly oriented fibers)
Composition: carbon matrix + 40% carbon fibers
Property Value in metric unit Value in US unit
Density 1.7 *10³ kg/m³ 106 lb/ft³
Flexural strength 250 MPa 36300 psi
Fracture modulus of elasticity 50 GPa 7250 ksi
Tensile strength 250 MPa 36300 psi

Related internal links


to Ceramic Matrix Composites (introduction)