Elastomer | ||||
Nitrile | ||||
Property | Value in metric unit | Value in US unit | ||
Density | 1.0 *10³ | kg/m³ | 62.4 | lb/ft³ |
---|---|---|---|---|
Tensile strength | 28 | MPa | 4060 | psi |
Elongation | 700 | % | 700 | % |
Glass transition temperature | -55 | ºC | -67 | ºF |
Maximum work temperature | 100 | ºC | 212 | ºF |
Electric resistivity | 102 | Ohm*m | 104 | Ohm*cm |
Dielectric constant | 13 | - | 13 | - |
Applications: hoses, gaskets, tanks lining, rolls coating.