Gold | ||||
Chemical composition: Au | ||||
Property | Value in metric unit | Value in US unit | ||
Density | 19.32 *10³ | kg/m³ | 1206 | lb/ft³ |
---|---|---|---|---|
Modulus of elasticity | 79 | GPa | 11450 | ksi |
Thermal expansion (20 ºC) | 14.2*10-6 | ºCˉ¹ | 7.9*10-6 | in/(in* ºF) |
Specific heat capacity | 129 | J/(kg*K) | 0.0308 | BTU/(lb*ºF) |
Thermal conductivity | 310 | W/(m*K) | 2149 | BTU*in/(hr*ft²*ºF) |
Heat of fusion | 6.3*104 | J/kg | 27 | BTU/lb |
Electric resistivity | 2.44*10-8 | Ohm*m | 2.44*10-6 | Ohm*cm |
Tensile strength (annealed) | 124 | MPa | 17985 | psi |
Elongation (annealed) | 45 | % | 45 | % |
Hardness (annealed) | 25 | HV | 25 | HV |
Melting point | 1064.4 | ºC | 1948 | ºF |
Annealing temperature | 300 | ºC | 575 | ºF |