Aliphatic solvent Hexane (n-Hexane, Hexyl hybride) | ||||
Chemical formula: CH3(CH2)4CH3 | ||||
Property | Value in metric unit | Value in US unit | ||
Density at 68°F (20°C) | 0.659 *10³ | kg/m³ | 41.2 | lb/ft³ |
---|---|---|---|---|
Viscosity at 68°F (20°C) | 0.31 | cP | 2.08*10-4 | lb/ft·s |
Surface tension at 77°F (25°C) | 0.01791 | N/m | 1.02*10-4 | lbf/in |
Vapor pressure at 77°F (25°C) | 150 | torr | 150 | torr |
Boiling point | 68.7 | ºC | 155.7 | ºF |
Melting Point | -95.3 | ºC | -139.5 | ºF |
Flash Point | -22 | ºC | -8 | ºF |
Autoignition temperature | 225 | ºC | 437 | ºF |
Dielectric constant at 77°F (25°C) | 1.88 | 1.88 | ||
Dipole moment at 77°F (25°C) | 0.08 | Debye | 0.08 | Debye |
Color | Colorless | Colorless |