Aromatic solvent Benzene
Chemical formula: C6H6
Property Value in metric unit Value in US unit
Density at 59°F (15°C) 0.879 *10³ kg/m³ 54.9 lb/ft³
Viscosity at 68°F (20°C) 0.65 cP 4.36*10-4 lb/ft·s
Vapor pressure at 77°F (25°C) 75 torr 75 torr
Boiling point 80.1 ºC 176.2 ºF
Melting Point 5.5 ºC 41.9 ºF
Flash Point -11 ºC 12 ºF
Autoignition temperature 498 ºC 928 ºF
Color Colorless Colorless