Property Value in metric unit Value in US unit
Density 1.0 *10³ kg/m³ 62.4 lb/ft³
Tensile strength 28 MPa 4060 psi
Elongation 700 % 700 %
Glass transition temperature -55 ºC -67 ºF
Maximum work temperature 100 ºC 212 ºF
Electric resistivity 102 Ohm*m 104 Ohm*cm
Dielectric constant 13 - 13 -
  • Excellent resistance to solvents, fuel, oil;
  • Good abrasion resistance;
  • Good resistance to acids;
  • Poor resistance to sunlight.

Applications: hoses, gaskets, tanks lining, rolls coating.