Engine oil SAE 5W-30 | ||||
Mineral based multigrade gasoline engine oil | ||||
Property | Value in metric unit | Value in US unit | ||
Density at 60°F (15.6°C) | 0.859 *10³ | kg/m³ | 53.6 | lb/ft³ |
---|---|---|---|---|
Kinematic viscosity at 104°F (40°C)/100°F (38°C) | 63.2 | cSt | 320 | SSU |
Kinematic viscosity at 212°F (100°C)/210°F (99°C) | 10.5 | cSt | 65 | SSU |
Viscosity index | 154 | 154 | ||
CCS viscosity at -22°F (-30°C) | 6400 | cP | 6400 | cP |
Flash point | 220 | ºC | 430 | ºF |
Pour Point | -36 | ºC | -35 | ºF |
Sulfated ash | 0.83 | % | 0.83 | % |
Neutralization No. (TBN-E) | 7.4 | 7.4 | ||
Color | 2 | 2 |