Pneumatic equipment lubricating and rust protection oil ISO 22

(submitted by the website administration)

Pneumatic equipment lubricating and rust protection oil ISO 22
Mineral paraffinic based oil with corrosion inhibitor
Property Value in metric unit Value in US unit
Density at 60°F (15.6°C) 0.855 *10³ kg/m³ 53.4 lb/ft³
Kinematic viscosity at 104°F (40°C) 23.0 cSt 23.0 cSt
Kinematic viscosity at 212°F (100°C) 4.4 cSt 4.4 cSt
Flash Point 230 ºC 446 ºF
Pour Point -29 ºC -20 ºF
Viscosity index 103 103
Color 0.5 0.5

Applications: air tools and other pneumatic equipment, indoor storage of metal parts, light bearings.