Chemical formula: CF4
Property Value in metric unit Value in US unit
Density of gas at 59°F (15°C) 3.72 kg/m³ 0.23 lb/ft³
Vapor pressure at 59°F (15°C) 3.65 MPa 529 psi
Boiling point -128 ºC -198 ºF
Melting point -184 ºC -298 ºF
Specific heat capacity (Cv) of gas at 86°F (30°C) 557 J/(kg*K) 0.133 BTU/(lb*ºF)
Specific heat capacity (Cp) of gas at 86°F (30°C) 659 J/(kg*K) 0.157 BTU/(lb*ºF)
Latent heat of vaporization 136 kJ/kg 58.5 BTU/lb