Thermoplastic | ||||
Polyamide (Nylon 6) | ||||
Property | Value in metric unit | Value in US unit | ||
Density | 1.13 *10³ | kg/m³ | 70.5 | lb/ft³ |
---|---|---|---|---|
Modulus of elasticity | 2.95 | GPa | 420 | ksi |
Tensile strength | 100 | MPa | 14500 | psi |
Elongation | 60 | % | 60 | % |
Flexural strength | 91 | MPa | 13000 | psi |
Thermal expansion (20 ºC) | 66*10-6 | ºCˉ¹ | 37*10-6 | in/(in* ºF) |
Thermal conductivity | 0.25 | W/(m*K) | 1.73 | BTU*in/(hr*ft²*ºF) |
Glass transition temperature | 50 | ºC | 122 | ºF |
Maximum work temperature | 110 | ºC | 230 | ºF |
Electric resistivity | 104 -107 | Ohm*m | 106 -109 | Ohm*cm |
Dielectric constant | 4.5 | - | 4.5 | - |
Applications: bushings, electrical plugs and sockets, gears, fibers for textiles, food packaging film, bearings, carpets.