Commercially pure nickel 270 (high purity nickel)

(submitted by the website administration)

Commercially pure nickel 270 (high purity nickel)
Chemical composition: Ni =99.9% min.
Property Value in metric unit Value in US unit
Density 8.89 *10³ kg/m³ 555 lb/ft³
Modulus of elasticity 207 GPa 30000 ksi
Thermal expansion (20 ºC) 13.3*10-6 ºCˉ¹ 7.4*10-6 in/(in* ºF)
Specific heat capacity 460 J/(kg*K) 0.11 BTU/(lb*ºF)
Thermal conductivity 86 W/(m*K) 597 BTU*in/(hr*ft²*ºF)
Electric resistivity 7.5*10-8 Ohm*m 7.5*10-6 Ohm*cm
Tensile strength (annealed) 345 MPa 50000 psi
Yield strength (annealed) 110 MPa 16000 psi
Elongation (annealed) 50 % 50 %
Liquidus temperature 1454 ºC 2650 ºF
Solidus temperature 1454 ºC 2650 ºF