Heat tranfer oil ISO 100
Mineral based oil
Property Value in metric unit Value in US unit
Density at 60°F (15.6°C) 0.890 *10³ kg/m³ 55.6 lb/ft³
Kinematic viscosity at 104°F (40°C) 90.2 cSt 90.2 cSt
Kinematic viscosity at 212°F (100°C) 10.6 cSt 10.6 cSt
Viscosity index 100 100
Flash point 267 ºC 512 ºF
Pour Point -9 ºC 14 ºF
Color 0.5 0.5
Thermal conductivity at 104°F (40°C) 0.0106 W/m*K 0.073 BTU*in/(hr*ft²*ºF)
Specific heat capacity at 104°F (40°C) 1950 J/(kg*K) 0.47 BTU/(lb*ºF)

Applications: heat transfer oil in closed circulation systems operating at temperatures up to 320ºC (620ºF), quenching oil for heat treating steels.