Main page
About us
Sliding Bearings Consulting
Advertising Opportunities
to Hydraulic oils
to Properties of fluids
(submitted by the website administration)
Hydraulic oil ISO 150 | ||||
Mineral based hydraulic oil | ||||
Property | Value in metric unit | Value in US unit | ||
Density at 60°F (15.6°C) | 0.882 *10³ | kg/m³ | 55.1 | lb/ft³ |
---|---|---|---|---|
Kinematic viscosity at 104°F (40°C) | 147 | cSt | 147 | cSt |
Kinematic viscosity at 212°F (100°C) | 14.6 | cSt | 14.6 | cSt |
Viscosity index | 98 | 98 | ||
Flash point | 286 | ºC | 547 | ºF |
Pour Point | -24 | ºC | -11 | ºF |
Aniline Point | 119 | ºC | 246 | ºF |
Color | max. 3.5 | max. 3.5 |