Low alloyed titanium alloy, Grade 12

(submitted by the website administration)

Low alloyed titanium, (Grade 12, Ti-0.3Mo-0.8Ni)
Chemical composition: O=0.25% max., Fe=0.3% max., Mo=0.3%, Ni=0.8%, Ti balance
Property Value in metric unit Value in US unit
Density 4.51 *10³ kg/m³ 282 lb/ft³
Modulus of elasticity 103 GPa 15000 ksi
Thermal expansion (20 ºC) 9.6*10-6 ºCˉ¹ 5.3*10-6 in/(in* ºF)
Specific heat capacity 544 J/(kg*K) 0.13 BTU/(lb*ºF)
Thermal conductivity 19 W/(m*K) 132 BTU*in/(hr*ft²*ºF)
Electric resistivity 56*10-8 Ohm*m 56*10-6 Ohm*cm
Tensile strength 517 MPa 75000 psi
Yield strength 448 MPa 65000 psi
Elongation 25 % 25 %
Hardness 88 HRB 88 HRB
Melting temperature 1660 ºC 3020 ºF
Beta Transus temperature 890 ºC 1634 ºF