Fluorocarbon solvent Tetrafluoromethane (Freon 14) | ||||
Chemical formula: CF4 | ||||
Property | Value in metric unit | Value in US unit | ||
Density of gas at 59°F (15°C) | 3.72 | kg/m³ | 0.23 | lb/ft³ |
---|---|---|---|---|
Vapor pressure at 59°F (15°C) | 3.65 | MPa | 529 | psi |
Boiling point | -128 | ºC | -198 | ºF |
Melting point | -184 | ºC | -298 | ºF |
Specific heat capacity (Cv) of gas at 86°F (30°C) | 557 | J/(kg*K) | 0.133 | BTU/(lb*ºF) |
Specific heat capacity (Cp) of gas at 86°F (30°C) | 659 | J/(kg*K) | 0.157 | BTU/(lb*ºF) |
Latent heat of vaporization | 136 | kJ/kg | 58.5 | BTU/lb |