Thread cutting oil
Mineral based oil
Property Value in metric unit Value in US unit
Density at 60°F (15.6°C) 0.917 *10³ kg/m³ 57.2 lb/ft³
Kinematic viscosity at 104°F (40°C) 23.1 cSt 23.1 cSt
Flash point 177 ºC 350 ºF
Pour Point -10 ºC 14 ºF


Applications: drilling, milling, threading, pipe-threading, broaching, boring, turning, tapping, engraving reaming, sawing.