Toughened acrylic adhesive
Two component (with initiator), toughened, high impact, high thermal resistance acrylic adhesive
Property Value in metric unit Value in US unit
Viscosity at 77°F (25°C) 17000 cP 0.355 lbf*sec/ft²
Fixture time 2 min 2 min
Full cure time 24 hrs 24 hrs
Maximum gap 0.5 mm 0.02 in
Shear strength, steel-to-steel 77°F (25°C) 20 MPa 2900 psi
Peel strength, steel-to-steel 77°F (25°C) 55 N/(25mm width) 12 PIW (lbf/inch width)
Min. service temperature -54 ºC -65 ºF
Max. service temperature 150 ºC 302 ºF