to Non-heat-treatable nickel-chromium-iron alloys
to Properties of nickel alloys
(submitted by the website administration)
| Non-heat-treatable Nickel-Chromium-Iron Alloy Hastelloy X | ||||
| Chemical composition: Cr=22%, Fe=18%, Mo=9%, W=0.6%, Co=1.5%, C=0.1%, Ni=47% | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 8.22*10³ | kg/m³ | 513 | lb/ft³ |
|---|---|---|---|---|
| Modulus of elasticity | 196 | GPa | 28500 | ksi |
| Thermal expansion (20 ºC) | 15.5*10-6 | ºCˉ¹ | 8.3*10-6 | in/(in* ºF) |
| Tensile strength (annealed) | 765 | MPa | 111000 | psi |
| Yield strength (annealed) | 380 | MPa | 55100 | psi |
| Elongation (annealed) | 44 | % | 44 | % |
| Liquidus temperature | 1355 | ºC | 2470 | ºF |
| Solidus temperature | 1260 | ºC | 2300 | ºF |