(submitted by the website administration)

Sintered aluminum alloy E
Chemical composition: Si=0.3%, Cu=2.0%, Mg=1%, Al+Al2O3 balance
Property Value in metric unit Value in US unit
Density 90% of theoretical density
Tensile strength (T6) 262 MPa 38000 psi
Yield strength (T6) 200 MPa 29000 psi
Elongation (T6) 3 % 3 %