to Quenching and heat transfer oils
to Properties of fluids

Quenching oil ISO 22

(submitted by the website administration)

Quenching oil ISO 22
Mineral based oil
Property Value in metric unit Value in US unit
Density at 60°F (15.6°C) 0.865 *10³ kg/m³ 54.0 lb/ft³
Kinematic viscosity at 104°F (40°C) 21.3 cSt 21.3 cSt
Kinematic viscosity at 212°F (100°C) 4.2 cSt 4.2 cSt
Viscosity index 100 100
Flash point 209 ºC 408 ºF
Pour Point -18 ºC -0.4 ºF
Color 0.5 0.5

Applications: general purpose heat treatment, quenching and heat transfer oil.

Related internal links


to Quenching and heat transfer oils
to Properties of fluids