| Single component high strength epoxy adhesive | ||||
| Single component high strength, free flowing epoxy adhesive | ||||
| Property | Value in metric unit | Value in US unit | ||
| Viscosity at 77°F (25°C) | 200000 | cP | 4.18 | lbf*sec/ft² |
|---|---|---|---|---|
| Cure time at 248°F (120°C) | 60 | min | 60 | min |
| Maximum gap | 0.5 | mm | 0.02 | in |
| Shear strength, steel-to-steel 77°F (25°C) | 34 | MPa | 5000 | psi |
| Peel strength, steel-to-steel 77°F (25°C) | 112 | N/(25mm width) | 25 | PIW (lbf/inch width) |
| Min. service temperature | -40 | ºC | -40 | ºF |
| Max. service temperature | 180 | ºC | 355 | ºF |