USA: AISI M2, UK: BM2, Sweden: 2722, Germany: 1.3341, Japan: SKH9 | ||||
Chemical composition: C=0.9%, Mn=0.3%, W=6%, Si=0.3%, Cr=4%, Mo=5%, V=2% | ||||
Property | Value in metric unit | Value in US unit | ||
Density | 8.17 *10³ | kg/m³ | 510.0 | lb/ft³ |
---|---|---|---|---|
Modulus of elasticity | 228 | GPa | 33000 | ksi |
Thermal expansion (20 ºC) | 11.0*10-6 | ºCˉ¹ | 6.1*10-6 | in/(in* ºF) |
Specific heat capacity | 418 | J/(kg*K) | 0.10 | BTU/(lb*ºF) |
Thermal conductivity | 24 | W/(m*K) | 167 | BTU*in/(hr*ft²*ºF) |
Annealing temperature | 870...890 | ºC | 1600...1630 | ºF |
Quenching temperature | 1150-1220 | ºC | 2100-2230 | ºF |
Tempering temperature | 540...650 | ºC | 1000...1200 | ºF |
Hardness (annealed) | 97 | RB | 97 | RB |
Hardness (hardened) | 66 | RC | 66 | RC |
Quenching medium | Oil, air or salt | |||
Hardening depth | High | |||
Resistivity to distortion | High | |||
Resistivity to cracking | Medium | |||
Machinability | Medium | |||
Toughness | Low | |||
Wear resistance | Very high |