Wrought copper alloy C36000 (Free-Cutting Brass) | ||||
Chemical composition: Zn=35.4%, Pb=3.1%, Cu=61.5% | ||||
Property | Value in metric unit | Value in US unit | ||
Density | 8.50 *10³ | kg/m³ | 531 | lb/ft³ |
---|---|---|---|---|
Modulus of elasticity | 96.5 | GPa | 14000 | ksi |
Thermal expansion (20 ºC) | 20.5*10-6 | ºCˉ¹ | 11.4*10-6 | in/(in* ºF) |
Specific heat capacity | 377 | J/(kg*K) | 0.090 | BTU/(lb*ºF) |
Thermal conductivity | 116 | W/(m*K) | 804 | BTU*in/(hr*ft²*ºF) |
Electric resistivity | 6.63*10-8 | Ohm*m | 6.63*10-6 | Ohm*cm |
Tensile strength (as fabricat.) | 338 | MPa | 49000 | psi |
Yield strength (as fabricated) | 124 | MPa | 18000 | psi |
Elongation (as fabricated) | 50 | % | 50 | % |
Shear strength (as fabricated) | 207 | MPa | 30000 | psi |
Hardness (as fabricated) | 68 | RF | 68 | RF |
Tensile strength (cold work) | 386 | MPa | 56000 | psi |
Yield strength (cold work) | 310 | MPa | 45000 | psi |
Elongation (cold work) | 20 | % | 20 | % |
Shear strength (cold work) | 228 | MPa | 33000 | psi |
Hardness (cold work) | 62 | RB | 62 | RB |
Annealing temperature | 425-600 | ºC | 800-1100 | ºF |
Liquidus temperature | 899 | ºC | 1650 | ºF |
Solidus temperature | 888 | ºC | 1630 | ºF |