Compression molded graphite

(submitted by the website administration)

Compression molded graphite
Chemical composition: carbon (C)
Property Value in metric unit Value in US unit
Density 1.76*10³ kg/m³ 110 lb/ft³
Modulus of elasticity 12 GPa 1740 ksi
Flexural strength 55 MPa 7980 psi
Compressive strength 90 MPa 13050 psi
Hardness 85 RB 10/100 85 RB 10/100
Thermal expansion (20 ºC) 2.2*10-6 ºCˉ¹ 1.2*10-6 in/(in* ºF)
Thermal conductivity 120 W/(m*K) 832 BTU*in/(hr*ft²*ºF)
Electric resistivity WG (with grain) 11*10-6 Ohm*m 11*10-4 Ohm*cm
Electric resistivity AG (against grain) 18*10-6 Ohm*m 18*10-4 Ohm*cm


Applications: contacts, crucibles for gas analysis, laboratory equipment.