Low thermal expansion isostatically pressed graphite
Chemical composition: carbon (C)
Property Value in metric unit Value in US unit
Density 1.73*10³ kg/m³ 108 lb/ft³
Modulus of elasticity 10.0 GPa 1450 ksi
Flexural strength 40 MPa 5800 psi
Compressive strength 90 MPa 13050 psi
Hardness 80 RB 10/100 80 RB 10/100
Thermal expansion (20 ºC) 2.7*10-6 ºCˉ¹ 1.5*10-6 in/(in* ºF)
Thermal conductivity 65 W/(m*K) 450 BTU*in/(hr*ft²*ºF)
Electric resistivity 17*10-6 Ohm*m 17*10-4 Ohm*cm


Applications: Laboratory equipment, crucibles for gas analysis, semiconductor crystals growing.