SubsTech     
SubsTech     

to Metal Matrix Composites (introduction)
to Properties of composites

Metal Matrix Composite Al-2%Cu-60% Al2O3 fiber

(submitted by the website administration)

Metal Matrix Composite Al-2%Cu-60% Al2O3 fiber
Composition: Aluminum alloy (2%Cu)+ 60 vol.% Al2O3 continuous fibers
Property Value in metric unit Value in US unit
Density 3.4 *10³ kg/m³ 212 lb/ft³
Modulus of elasticity (long.) 240 GPa 34800 ksi
Modulus of elasticity (trans.) 160 GPa 23200 ksi
Tensile strength (longitude.) 1500 MPa 217550 psi
Compressive strength (long.) 3400 MPa 493100 psi