Metal matrix Composite Duralcan F3S.20S
Composition: Aluminum alloy 359 + 20%SiC particles
Property Value in metric unit Value in US unit
Density 2.85 *10³ kg/m³ 178 lb/ft³
Modulus of elasticity 98.6 GPa 14300 ksi
Tensile strength (T6) 359 MPa 52070 psi
Yield strength (T6) 338 MPa 49020 psi
Elongation (T6) 0.40 % 0.40 %
Hardness 77 HRB 77 HRB
Thermal expansion (20 ºC) 20.7*10-6 ºCˉ¹ 11.5*10-6 in/(in* ºF)
Thermal conductivity 144 W/(m*K) 999 BTU*in/(hr*ft²*ºF)