Silver-ABA
Chemical composition: Ag=92.75%, Cu=5.0%, Ti=1.25%, Al-1.0%
Property Value in metric unit Value in US unit
Density 10.0 *10³ kg/m³ 5.27 Troy oz/in³
Modulus of elasticity 77 GPa 11170 ksi
Thermal expansion (20 ºC) 2.07*10-5 ºCˉ¹ 1.15*10-5 in/(in* ºF)
Thermal conductivity 344 W/(m*K) 2385 BTU*in/(hr*ft²*ºF)
Electrical resistivity 2.2*10-8 Ohm*m 2.2*10-6 Ohm*cm
Tensile strength 136 MPa 20000 psi
Yield strength 282 MPa 41000 psi
Elongation 37 % 37 %