High temperature compression molded carbon-graphite
Chemical composition: carbon (C)
Property Value in metric unit Value in US unit
Density 1.8*10³ kg/m³ 112 lb/ft³
Flexural strength 59 MPa 8555 psi
Compressive strength 152 MPa 22040 psi
Hardness (Shore) 80 HS 80 HS
Thermal expansion (20 ºC) 2*10-6 ºCˉ¹ 1.1*10-6 in/(in* ºF)
Thermal conductivity 69 W/(m*K) 478 BTU*in/(hr*ft²*ºF)
Max. service temperature in air 649 °C 1200 ºF