to Metal Matrix Composites (introduction)
to Properties of composites

Metal Matrix Composite 2124-25%SiC

(submitted by the website administration)

Metal Matrix Composite 2124-25%SiC
Composition: Aluminum alloy 2124 + 25%SiC particles
Property Value in metric unit Value in US unit
Density 2.88*10³ kg/m³ 180 lb/ft³
Modulus of elasticity 115 GPa 16680 ksi
Tensile strength 650 MPa 94270 psi
Yield strength 480 MPa 69620 psi

Related internal links


to Metal Matrix Composites (introduction)
to Properties of composites