 Permanent mold casting (gravity die casting) is a casting process involving pouring a molten metal by gravity into a steel (or cast iron) mold.
The permanent mold casting is similar to the sand casting process . In distinction from sand molds, which are broken after each casting a permanent mold may be used for pouring of at least one thousand and up to 120,000 casting cycles with the rate 5-100 castings/hour.
Manufacturing metal mold is much more expensive than manufacturing molds for Sand casting or investment  casting process mold. Minimum number of castings for profitable use of a permanent mold is dependent on the complexity of its shape.
 
 Ferrous and no-ferrous metals and alloys are cast by the permanent mold casting process: Aluminum alloys, Copper alloys, Magnesium alloys, zinc alloys, steels and Cast irons.
 
Advantages of permanent mold casting process are determined by relatively high cooling rate caused by solidification in metallic mold:
Disadvantages of permanent mold casting:
 