SubsTech     
SubsTech     
Command disabled: index

to Metal Matrix Composites (introduction)
to Properties of composites

Metal Matrix Composite 2124-25%SiC

(submitted by the website administration)

Metal Matrix Composite 2124-25%SiC
Composition: Aluminum alloy 2124 + 25%SiC particles
Property Value in metric unit Value in US unit
Density 2.88*10³ kg/m³ 180 lb/ft³
Modulus of elasticity 115 GPa 16680 ksi
Tensile strength 650 MPa 94270 psi
Yield strength 480 MPa 69620 psi

Related internal links

metal_matrix_composite_2124-25_sic.txt · Last modified: 2023/12/14 by dmitri_kopeliovich