Chemical composition: Ni=20%, Fe=1.0%,Mn=0.9%, Nb=1.0%, Cu=balance
Property Value in metric unit Value in US unit
Density 8.94 *10³ kg/m³ 558 lb/ft³
Modulus of elasticity 138 GPa 20000 ksi
Thermal expansion (20 ºC) 16.4*10-6 ºCˉ¹ 9.1*10-6 in/(in* ºF)
Specific heat capacity 377 J/(kg*K) 0.090 BTU/(lb*ºF)
Thermal conductivity 36.8 W/(m*K) 256 BTU*in/(hr*ft²*ºF)
Electric resistivity 27.8*10-8 Ohm*m 27.8*10-6 Ohm*cm
Tensile strength (sand cast) 517 MPa 75000 psi
Yield strength (sand cast) 379 MPa 55000 psi
Elongation (sand cast) 10 % 10 %
Hardness (sand cast) 150 HB(500) 150 HB(500)
Liquidus temperature 1199 ºC 2190 ºF
Solidus temperature 1149 ºC 2100 ºF

Related internal links

Related external links

cast_copper_alloy_c96300_copper-nickel.txt · Last modified: 2012/06/02 by dmitri_kopeliovich
Promote in SubsTech       Creative Commons License Except where otherwise noted, this work is licensed under a Creative Commons Attribution-Noncommercial-Share Alike 3.0 License