SubsTech     
SubsTech     

to Cast copper-nickel alloys and Nickel Silvers
to Properties of copper alloys

Cast copper alloy C97800 (Nickel-Silver 25% Ni)

(submitted by the website administration)

Cast copper alloy C97800 (Nickel-Silver 25% Ni)
Chemical composition: Ni=25.5%, Zn=2.5%, Sn=4.8%, Pb=1.8% Cu=balance
Property Value in metric unit Value in US unit
Density 8.86 *10³ kg/m³ 553 lb/ft³
Modulus of elasticity 131 GPa 19000 ksi
Thermal expansion (20 ºC) 17.5*10-6 ºCˉ¹ 9.7*10-6 in/(in* ºF)
Specific heat capacity 377 J/(kg*K) 0.090 BTU/(lb*ºF)
Thermal conductivity 25.4 W/(m*K) 176 BTU*in/(hr*ft²*ºF)
Electric resistivity 38.5*10-8 Ohm*m 38.5*10-6 Ohm*cm
Tensile strength (sand cast) 310 MPa 45000 psi
Yield strength (sand cast) 165 MPa 24000 psi
Elongation (sand cast) 20 % 20 %
Fatigue strength (sand cast) 107 MPa 16000 psi
Hardness (sand cast) 80 HB(500) 80 HB(500)
Liquidus temperature 1180 ºC 2156 ºF
Solidus temperature 1140 ºC 2084 ºF

Related internal links

Related external links

cast_copper_alloy_c97800_nickel-silver_25_ni.txt · Last modified: 2012/06/02 by dmitri_kopeliovich
Promote in SubsTech       Creative Commons License Except where otherwise noted, this work is licensed under a Creative Commons Attribution-Noncommercial-Share Alike 3.0 License