Cast copper alloy C96400 (70-30 Copper-Nickel)
Chemical composition: Ni=30%, Fe=0.9%, Nb=1.0%, Cu=balance
Property Value in metric unit Value in US unit
Density 8.94 *10³ kg/m³ 558 lb/ft³
Modulus of elasticity 145 GPa 21000 ksi
Thermal expansion (20 ºC) 16.2*10-6 ºCˉ¹ 9.0*10-6 in/(in* ºF)
Specific heat capacity 377 J/(kg*K) 0.090 BTU/(lb*ºF)
Thermal conductivity 28.5 W/(m*K) 197 BTU*in/(hr*ft²*ºF)
Electric resistivity 35.7*10-8 Ohm*m 35.7*10-6 Ohm*cm
Tensile strength (sand cast) 469 MPa 68000 psi
Yield strength (sand cast) 255 MPa 37000 psi
Elongation (sand cast) 28 % 28 %
Fatigue strength (sand cast) 124 MPa 18000 psi
Hardness (sand cast) 140 HB(3000) 140 HB(3000)
Liquidus temperature 1238 ºC 2260 ºF
Solidus temperature 1117 ºC 2140 ºF

Related internal links

Related external links

cast_copper_alloy_c96400_70-30_copper-nickel.txt · Last modified: 2012/06/02 by dmitri_kopeliovich
Promote in SubsTech       Creative Commons License Except where otherwise noted, this work is licensed under a Creative Commons Attribution-Noncommercial-Share Alike 3.0 License